﻿"Sample type";"Specific weight of absorbed oxygen at 420 °C, g/cm2";"Specific weight of absorbed oxygen at 535 °C, g/cm2"
Lead;1.09×10–2;3.64×10–2
"Alloy with equal mass fractions of Pb and Bi";1.95×10–2;4.87×10–2
Bismuth;2.27×10–2;6.17×10–2