Microstructure of the fuel composition UO2+Mg in the cross-section of the artificial defect after testing the FE sample in the water for 365 days: away from the through defect (a) and in the zone of corrosion interaction with the aqueous medium (b).

 
 
  Part of: Ivanov SN, Porollo SI, Baranaev YD, Timofeev VF, Kharizomenov YV (2019) Corrosion tests in water of fuel elements irradiated in the world’s first NPP reactor. Nuclear Energy and Technology 5(4): 337-343. https://doi.org/10.3897/nucet.5.48427