General cross-sectional view of the FE fragments with U-Mo+Mg fuel (a) and UO2+Mg fuel (b) after testing in water for 430 and 365 days, respectively (arrows indicate the contour of the outer surface of the artificial defect prior to corrosion testing).

 
 
  Part of: Ivanov SN, Porollo SI, Baranaev YD, Timofeev VF, Kharizomenov YV (2019) Corrosion tests in water of fuel elements irradiated in the world’s first NPP reactor. Nuclear Energy and Technology 5(4): 337-343. https://doi.org/10.3897/nucet.5.48427